Capsulization


Reading time ( words)

Since lead-free implementation, concerns about tin whiskers have intensified. For the past 12 years, studies and research by various laboratories and organizations have delivered burgeoning reports and papers, and my column has devoted an entire series to this subject. This article aims to capsulize the important areas of the subject. (Note: For expression, “whisker” is used as both noun and verb.)

The tin whisker issue and its potential mishaps have been recognized for more than six decades in electronic, electrical, and industrial applications. Some metals are prone to whiskering, or protruding from the surface of the substrate. In addition to tin, the metals that have exhibited whiskers include zinc, cadmium, silver, gold, aluminum, copper, lead, and others.

The whiskering phenomenon is distinct and unique. It is the result of a process different from other known phenomena (e.g., dendrites). And tin whisker and tin pest are separate metallurgical phenomena (SMT Magazine, May 2013). However, whiskers share commonality with dendrites in two aspects: Both are the result of a physical metallurgical process, thus following the science of physical metallurgy; and both could cause a product failure.

Uncertainty about tin whisker growth is most insidious. Stock markets do not like uncertainty, nor does the electronics industry. Our effort is to alleviate the uncertainty.

Practical Criteria

As some metals can whisker when accommodating conditions are met, the goal should be set with the differentiation between whisker-resistant and whisker-proof.

Overall, for testing or evaluation of the whisker propensity of a system, the key questions to be addressed are, is the system whisker-prone or whisker-resistant (not whisker-proof), and how does the system’s whisker resistance stand in reference to the intended benchmark?

Read the full article here.


Editor's Note: This article originally appeared in the July 2014 issue of SMT Magazine.

Share




Suggested Items

Book Excerpt: 'The Printed Circuit Assembler’s Guide to… Solder Defects'

06/07/2022 | I-Connect007 Editorial Team
Solder defects in surface-mount technology (SMT) assembly have been an issue for decades. Further, the combined challenges of Pb-free soldering and ever-increasing miniaturization have resulted in new or exacerbated defects in electronics assembly, but there are proven ways to avoid defects. This book will be especially beneficial to PCB assemblers in improving their assembly processes and the reliability of the end-product, eliminating field failures, and reducing costs.

Dave Hillman on Living Your Passion

03/29/2022 | Barry Matties, I-Connect007
Barry Matties leads this engaging retrospective conversation with Dave Hillman, a Fellow, Materials and Process engineer at Collins Aerospace, who talks about mentorship, pandemic changes, and solder. “Soldering is soldering,” Dave says. “But how we do that keeps evolving in response to the new technologies and smaller packages.” What’s the key to his success and longevity? “Find your passion.” Here’s how he’s done it.

Real Time with… IPC APEX EXPO 2022: Blackfox Mixes It Up with Training Opportunities

01/11/2022 | Andy Shaughnessy, Design007 Magazine
Andy Shaughnessy speaks with Jamie Noland, master IPC trainer and marketing manager for Blackfox Institute, about current and upcoming training opportunities and what you can expect from them at the show. Blackfox has expanded its offerings to reach a wider audience, including some very basic classes for beginners.



Copyright © 2022 I-Connect007. All rights reserved.